Magnesium is OEM.......it reacts the quickest to water chemistry and is a better conductor of electrical current (which is the reason it is a great sacrificial rod)
Aluminum will last longer but can accumulate deposits on the rod which can make it harder to remove.
If an anode rod has lasted 4 yrs. I would be concerned how well it was providing corrosion protection...it is suppose to deteriorate vs the steel tank Suburban uses.
Aluminum will last longer but can accumulate deposits on the rod which can make it harder to remove.
If an anode rod has lasted 4 yrs. I would be concerned how well it was providing corrosion protection...it is suppose to deteriorate vs the steel tank Suburban uses.