Mr__C
Nov 21, 2022Explorer
Anode Rod Wear
What would cause severe wear to the rod at the connection end? Almost no wear on the rest of the rod. I use teflon tape on the threads. Two brand new rods, two years in a row.
MFL wrote:I agree, I switched to magnesium because I was getting a lot of the slimy aluminum compound in the bottom of the tank. Changing to magnesium took care of that issue.
Those rods look good, if each had a years use. You can easily get another year of use out of either of those. Looks like 80% or more left, and should be able to use down to 25-50% with still good protection.
Your money, you decide, but changing to aluminum not necessary.