BenK wrote:
That is always one thing to look for with such high PSI's, as there is
always the 'other side' of the mechanism that generates that PSI
now wonder if the organic amines is first softened or changed by it to then see cavitation that finalizes the attack?
Once the DLC coating is compromised, the process of ablation is pretty rapid and can do so with many possible mechanisms.
Straight wear.
Cavitation?
You name it.... all the way to 2,000 bars.
The first metal fragment probably initiate the final self destruct sequence.
http://www.youtube.com/watch?v=dd6VXLHKIUM