Veebyes wrote:
If you are into a restoration that deep, use marine grade plywood & give that a coating of an additional preservative so that you will never be doing the job again.
Real marine grade plywood is incredibly expensive ! (Hint: You will know it it the "real thing" if it is sold in mm thickness and NOT inches !) 1/4-3/8 ACX or BCX is more than adequate for the job.
Any additional coating should NOT be required if the roofing material is doing its job !